Aluminium-Druckguss-Teil des Wärmetauschers
1 / 8
Aluminium-Druckguss-Teil des Wärmetauschers
Aluminium-Druckguss-Teil des Wärmetauschers
Zuhause> Produkt-Liste> Maschinenteile> Maschinenteile Gehäuse> Aluminium-Druckguss-Teil des Wärmetauschers

Aluminium-Druckguss-Teil des Wärmetauschers

Zahlungsart: T/T
Incoterm: FOB,CFR,CIF,FCA
$11,300.00   —  $5,600,000.00 /Set

Produktbeschreibung

Produkteigenschaften

ModellBL031

MarkeKEINER

TypeWindscreen Wiper System

MaterialAluminum

Muffler TypeCenter Muffler

DeckDouble

Surface FinishElectrophoresis Coating

Cavity Number2

Weight200g-3000g

Lieferfähigkeit & Zusatzinformationen

VerpakungKarton, PE-Palette

Produktivität5000/MONTH

TransportOcean,Land,Air

Ort Von ZukunftNingbo.

Unterstützung über150000/MONTH

Zertifikate IATF16949:2016,ISO14001:2015,ISO45001:2018

HS-Code7616991090

HafenNINGBO,SHANGHAI

ZahlungsartT/T

IncotermFOB,CFR,CIF,FCA

Verpackung & Lieferung

Verkaufseinheiten:
Piece/Pieces
Pakettyp:
Karton, PE-Palette

Produktbeschreibung

Aluminum die Casting part of Heat Exchanger, it is a new part developed, the part is the major housing for the motor . the cavity number for this part is 1, according to the required tolerance and dimensions, the difficult point of this part is the CNC machining work,


The CNC machining work is finished on high precision machining center, we used BROTHER machining center, the accuracy can be up to 0.005 mm. The fourth rotary table we used is NIKKEN. Prior to machining, the part will be shot peeninged, or called shot blasting, shot peening is to make the appearance of the part more consistency, eliminating the mark of deburring more or less. What's more, shot blasting also can make the mechanical property better.


In die casting process, should pay attention to gas bulging bubble
Features: skin of casting, formed gas bulging bubble.

Causes
1, mold temperature is too high.
2, the filling speed is too high, the metal flow into the gas too much.
3, coating gas, excessive amount of unburned, before pouring, the volatile gas enclosed in the surface layer of the casting.
4, the exhaust is not smooth.
5, premature opening.
6, alloy smelting temperature is too high.


Exclusion measures
1. Cooling mold to working temperature.
2, reduce the injection speed, avoid eddy gas inclusion.
3, the small air quantity amount of coating, thin and uniform, then die out.
4. Cleaning and adding overflow tank and exhaust duct.
5, adjust the mold leaving time.
6. Dressing smelting process.

The material required for this part is ADC-12, a Japanese standard aluminum, very common material applied in high pressure die casting . The material should conform to standard of JIS H 5302-2000.


Aluminum Die Casting Heat Exchanger Parts : Aluminum Casting of Heat Exchanger
Die Casting Machine: 550 ton
1 part per die
Material: ADC-12
Product Dimensions: 367mm*288.6mm*48mm
Casting Precision: Grade GB-CT3
Machining Precision Axle hole: ±0.07mm
Technological Process: Die casting, Degate, Burring, Polish,CNC Milling, Cleaning, Packing, Delivery
Control Measure: First item inspection, Routing inspection, Final item inspection, Incoming test and Outgoing quality control
Inspection Equipment: CMM and Screw Gauge
Surface Treatment: Polish
Certificate: IATF16949:2016,ISO14001:2015,ISO45001:2018
Lead Time: 30-35 days
Trade Term: FOB Ningbo

BOLANG PLANTDIE CASTING MACHINE

CNC work shop


CMM facility

heiße Produkte

Zuhause> Produkt-Liste> Maschinenteile> Maschinenteile Gehäuse> Aluminium-Druckguss-Teil des Wärmetauschers

Copyright ©2024 NINGBO ZHENHAI BOLANG METAL PRODUCT FACTORYAlle Rechte vorbehalten

Anfrage versenden
*
*

We will contact you immediately

Fill in more information so that we can get in touch with you faster

Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.

senden